Mechanical Properties Metric English Comments
Tensile Modulus 3.66 GPa
531 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Tensile Modulus 3.66 GPa
531 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Tensile Modulus 3.66 GPa
531 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Tensile Modulus 3.66 GPa
531 ksi
ASTM 638
NOVA Chemicals Dylark® 432 High-Heat Styrenic Copolymer
Product Description and Features: Styrenic copolymer with excellent heat resistance and good modulus. Resin designed for use as an additive to promote adhesion and compatibility in compounding of ..
Tensile Modulus 3.66 GPa
531 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI
LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare.
Tensile Modulus 3.66 GPa
531 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP
LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized.
Tensile Modulus 3.66 GPa
531 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..