Mechanical Properties Metric English Comments
Tensile Modulus 3.29 GPa
477 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid (PVC, Rigid)
** NOTE: UL REGULATORY LISTING PENDINGInformation provided by PolyOne
Tensile Modulus 3.29 GPa
477 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP COLORCOMP EX10304C PEI (Asia Pacific)
LNP* Colorcomp* EX10304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS Technol..
Tensile Modulus 3.29 GPa
477 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon
LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized.
Tensile Modulus 3.29 GPa
477 ksi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
CRP Technology Windform® GT Polyamide Glass Composite
Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter...
Tensile Modulus 3.29 GPa

@Temperature -60.0 °C
477 ksi

@Temperature -76.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Tensile Modulus 3.29 GPa

@Temperature -60.0 °C
477 ksi

@Temperature -76.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Tensile Modulus 3.29 GPa

@Temperature -10.0 °C
477 ksi

@Temperature 14.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..