Mechanical Properties Metric English Comments
Tensile Modulus 3.06 GPa
444 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY FXW749SK ASA
Sparkle VisualFx ASA Resin - Weatherable
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK
LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific)
LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK
LNP* LUBRICOMP* LL004E is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 3.06 GPa
444 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 3.06 GPa
444 ksi
ISO R527 Type 1
Hexcel® HexPly® 1454 125°C Curing Epoxy Matrix
HexPly® 1454 is a self-extinguishing epoxy resin system with very high self adhesion properties. It has good handling and is tolerant of a wide range of processing conditions. HexPly® 1454 is idea..
Tensile Modulus 3.06 GPa
444 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne