Polymer Property : Tensile Modulus = 2640 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.20 - 18.2 GPa
754 - 2640 ksi
MD
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic
Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co..