Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.20 - 18.2 GPa | 754 - 2640 ksi | MD |
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co.. |