Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.82 GPa | 264 ksi | ISO 527 |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Geon™ L4605 Red 7640 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 1mm/min |
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo.. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | ISO 527-2 |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Tensile Modulus | 1.82 GPa @Thickness 3.20 mm |
264 ksi @Thickness 0.126 in |
Injection Molded; ISO 527-2 |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Tensile Modulus | 1.82 GPa @Thickness 3.20 mm |
264 ksi @Thickness 0.126 in |
Injection Molded; ISO 527-2 |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.82 GPa | 264 ksi | Storage |
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy Product Description: EPO-TEK® OG116-31 is a single component, UV curable epoxy adhesive and encapsulant, designed for PCB and circuit assembly applications found in semiconductor, computer, medical.. |