Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.34 GPa | 2515 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |