Polymer Property : Tensile Modulus = 17.34 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 17.34 GPa
2515 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.