Mechanical Properties Metric English Comments
Tensile Modulus 0.172 - 0.345 GPa
25.0 - 50.0 ksi
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System
Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or inciden..
Tensile Modulus 0.172 GPa
25.0 ksi
TM R050-36
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..
Tensile Modulus 0.172 GPa
25.0 ksi
ASMT D638 Die C
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..