Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.172 - 0.345 GPa | 25.0 - 50.0 ksi | |
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or inciden.. |
|||
Tensile Modulus | 0.172 GPa | 25.0 ksi | TM R050-36 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Tensile Modulus | 0.172 GPa | 25.0 ksi | ASMT D638 Die C |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |