Polymer Property : Tensile Modulus = 231 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 231 GPa
33500 ksi
Typical fiber property; Chord 6000-1000
Hexcel® HexTow™ AS4C Carbon Fiber
HexTow™ AS4C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated..
Tensile Modulus 231 GPa
33500 ksi
Typical fiber property; Chord 6000-1000
Hexcel® HexTow™ AS4 Carbon Fiber
HexTow™ AS4 carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. The fiber has been surface treated a..