Material Notes:
HexTow™ AS4C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. Suggested for use in weaving, prepregging, filament winding, pultrusion, and molding compounds.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Filament Diameter 6.9 µm
6.9 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2263 MPa
328200 psi
Typical epoxy composite property
4410 MPa
640000 psi
Typical fiber property
Elongation at Break 1.8 %
1.8 %
Calculated from tow test data
Tensile Modulus 143 GPa
20700 ksi
Typical epoxy composite property
231 GPa
33500 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 128 GPa
18600 ksi
Typical epoxy composite property
Shear Strength 124 MPa
18000 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 1.25
12K
2.5
6K
5
3K
Fiber Volume (%) 62
Filament Shape Round
Tow Cross-Sectional Area (mm2) 0.11
3K
0.22
6K
0.45
12K
Twist None
Weight/Length (g/m) 0.2
3K
0.4
6K
0.8
12K