Polymer Property : Tensile Modulus = 203 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.25 - 1.40 GPa

@Thickness 2.00 mm
181 - 203 ksi

@Thickness 0.0787 in
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM ..
Tensile Modulus 1.20 - 1.40 GPa
174 - 203 ksi
TD; ISO 527-3
Borealis BorPURE™ RB501BF Polypropylene Copolymer
BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives..
Tensile Modulus 1.00 - 1.40 GPa
145 - 203 ksi
DIN 53 457
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Tensile Modulus 1.25 - 1.40 GPa

@Thickness 2.00 mm,
Temperature 23.0 °C
181 - 203 ksi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.