Borealis BorPURE™ RB501BF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name BorPURE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPURE™ RB501BF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives: BorPure™ RB501BF contains no slip, antiblock, antistatic additives or nucleating additives.Information provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
2.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
8.1 g/10 min

@Load 5.00 kg,
Temperature 230 °C
8.1 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 80 - 100 %
80 - 100 %
ISO 527-3
Tensile Modulus 1.10 - 1.30 GPa
160 - 189 ksi
MD; ISO 527-3
1.20 - 1.40 GPa
174 - 203 ksi
TD; ISO 527-3
Film Tensile Strength at Break, MD 150 - 180 MPa
21800 - 26100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 136 - 142 °C
277 - 288 °F
DSC; ISO 3146
Optical Properties Metric English Comments
Haze <= 1.8 %
<= 1.8 %
ASTM D1003
Gloss >= 90 %
>= 90 %
45° of arc; ASTM D2457