Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.24 GPa | 1630 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66 LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 11.2 GPa @Temperature -140 °C |
1630 ksi @Temperature -220 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |