Mechanical Properties Metric English Comments
Tensile Modulus 15.6 GPa
2260 ksi
ASTM D638
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Tensile Modulus 15.6 GPa
2260 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 15.6 GPa
2260 ksi
ASTM D638
Plenco 6343 Phenolic, Granular, Compression Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Tensile Modulus 15.6 GPa
2260 ksi
ISO 527-1/-2
DSM Arnite® TV4 290 PBT-GF50
50% Glass Reinforced
Tensile Modulus 15.6 GPa
2260 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)  (Unverified Data**)