Plenco 6343 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6343 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recognized under component file E40654. 06343 is available in natural color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.850 g/cc
0.0307 lb/in³
ASTM D1895
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.045 %
0.045 %
ASTM D570
Linear Mold Shrinkage 0.00285 cm/cm
0.00285 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 71
71
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 0.31 %
0.31 %
ASTM D638
Tensile Modulus 15.6 GPa
2260 ksi
ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 12.1 GPa
1750 ksi
ASTM D790
Compressive Strength 169 MPa
24500 psi
ASTM D695
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.183 J/cm²
0.871 ft-lb/in²
ASTM D256
Impact 69
69
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 W/m-K

@Temperature 100 °C
3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 225 °C
437 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 43 %
43 %
ASTM D2863
Shrinkage 0.040 %
0.040 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+13 ohm-cm
1.50e+13 ohm-cm
ASTM D247
Dielectric Constant 4.6
4.6
ASTM D150
Dielectric Strength 17.7 kV/mm
450 kV/in
Short Time; ASTM D149
Dissipation Factor 0.0172
0.0172
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638