Mechanical Properties Metric English Comments
Tensile Modulus 138 GPa
20000 ksi
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S(HT) Powdered Metal
Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-85(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Modulus 138 GPa
20000 ksi
PSM Industries Pacific Sintered Metals Nickel Iron FN-250-S Powdered Metal
Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0200-20Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Modulus 138 GPa
20000 ksi
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S(HT) Powdered Metal
Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0208-130HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Modulus 138 GPa
20000 ksi
ASTM D3039
Greene Tweed WRâ„¢ 525 PEEK, Carbon Filled
WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca..
Tensile Modulus 138 GPa
20000 ksi
0°; RT
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, Annealed
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, Extra Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, Extra Spring
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
Eagle Brass 725 Copper Nickel Tin, Spring
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Modulus 138 GPa
20000 ksi
ASTM E8
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing
Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for ..
Tensile Modulus 138 GPa
20000 ksi
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division..