Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing

Category Metal , Ferrous Metal , Tool Steel , Air-Hardening Steel , Cold Work Steel
Manufacturer 3D Systems Corporation
Trade Name LaserForm™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for producing rapid tooling inserts quickly and inexpensively. Specific applications include complex tooling inserts for injection molding and die casting, small/complex metal parts, and short run manufacturing. Tolerances may be a problem so post-machining may be needed. If this is the case then machining stock should be added the CAD drawings.For use with Sinterstation® HiQ™ series and other SLS® systems.ApplicationsComplex tooling inserts for injection molding and die-castingConformal cooling or heating channels integrated into tool designsSmaller and complex geometry metal partsLow volume metal part manufacturingProperty data is for sintered and infiltrated parts.Information provided by Axis Prototypes.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell C 10 - 20
10 - 20
as-infiltrated; polished surface; ASTM E18
39
39
heat treated; ASTM E18
Tensile Strength at Break 610 MPa
88500 psi
ASTM E8
Tensile Strength, Yield 470 MPa
68200 psi
0.2% offset; ASTM E8
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM E8
Tensile Modulus 138 GPa
20000 ksi
ASTM E8
Compressive Yield Strength 480 MPa
69600 psi
ASTM E8
Thermal Properties Metric English Comments
CTE, linear 7.45 µm/m-°C
4.14 µin/in-°F
ASTM E831
Thermal Conductivity 39.0 W/m-K

@Temperature 215 °C
271 BTU-in/hr-ft²-°F

@Temperature 419 °F
ASTM E457
Descriptive Properties Value Comments
Color Light Bronze