Tensile Modulus 0.600 - 0.800 GPa

@Temperature 100 °C
87.0 - 116 ksi

@Temperature 212 °F
DIN 53457
Zell-Metall Engineering Plastics Zellamid 1115
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..