Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.600 - 0.800 GPa @Temperature 100 °C |
87.0 - 116 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |