Mechanical Properties Metric English Comments
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EA-LR43 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EP-521 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EP-610AS ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON RP-4020 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON RP-4040 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON RP-5000 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON RP-5000AS EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EP-620 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Tensile Modulus 0.490 - 0.784 GPa
71.1 - 114 ksi
ASTM D638
Daikin NEOFLON EP-541 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..