Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.490 GPa | 71.1 ksi | |
Kuraray HYBRAR® PH5 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.490 GPa | 71.1 ksi | |
Kuraray HYBRAR® PH1 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Tensile Modulus | 0.490 GPa @Temperature 120 °C |
71.1 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8202CQ PA6 (Dry) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Tensile Modulus | 0.490 - 0.784 GPa | 71.1 - 114 ksi | ASTM D638 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |