Mechanical Properties Metric English Comments
Tensile Modulus 1.78 GPa

@Temperature 23.0 °C
258 ksi

@Temperature 73.4 °F
50 mm/min; ASTM D638
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Tensile Modulus 1.78 GPa
258 ksi
1mm/min
Eastman Tenite 383A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Tensile Modulus 1.78 GPa

@Thickness 3.20 mm
259 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
LG Chemical HIPS 60HRI PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che..
Tensile Modulus 1.78 GPa
258 ksi
50 mm/min; ASTM D638
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..
Tensile Modulus 1.78 GPa
258 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MD000AP PP
LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.
Tensile Modulus 1.78 GPa
258 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Tensile Modulus 1.78 GPa
258 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic
LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked.
Tensile Modulus 1.78 GPa
258 ksi
ASTM D638
Styrolution Terluran® EHI-4 NR ABS Extrusion Application
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Tensile Modulus 1.78 GPa
258 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP
LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact.
Tensile Modulus 1.78 GPa
258 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Tensile Modulus 1.78 GPa
258 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Tensile Modulus 1.78 GPa
258 ksi
Storage
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy
Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE..