Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.78 GPa @Temperature 23.0 °C |
258 ksi @Temperature 73.4 °F |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 1mm/min |
Eastman Tenite 383A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | ASTM D638 |
Styrolution Terluran® EHI-4 NR ABS Extrusion Application Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Tensile Modulus | 1.78 GPa | 258 ksi | Storage |
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE.. |