Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, high scratch resistance and good UV resistance are required.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, South America and North America Features: Good Surface FinishHigh Impact ResistanceHigh Scratch ResistanceLow to No FoggingLow to No OdorLow VOC Uses: Automotive Instrument PanelAutomotive Interior Parts Automotive Interior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Melt Flow 13 g/10 min
13 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527-2
Tensile Modulus 1.78 GPa
258 ksi
Secant; ISO 527-2
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Charpy Impact, Notched 0.399 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.798 J/cm²

@Temperature 0.000 °C
3.80 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
1.49 J/cm²

@Temperature 22.8 °C
7.10 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A