Tensile Modulus 1.36 GPa
197 ksi
same value from ASTM and ISO test.
BASF Capron® 8202C HS Nylon 6 (Conditioned)  (discontinued **)
Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i..
Tensile Modulus 1.36 GPa
197 ksi
Hybrid Plastics Nanoreinforced® PM 1215 Polyimide
The homogeneous dispersion of POSS® cages within polyimide provides enhanced control over chain dynamics which increases the toughness and damage tolerance over conventional polyimide. The chemic..
Tensile Modulus 1.36 GPa
197 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP
SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS..
Tensile Modulus 1.36 GPa
197 ksi
Storage
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive
Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p..
Tensile Modulus 1.36 GPa
197 ksi
1 mm/min
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient..
Tensile Modulus 1.36 GPa
197 ksi
1 mm/min
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Dry)
Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food..
Tensile Modulus 1.36 GPa
197 ksi
ASTM Test
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.
Tensile Modulus 1.36 GPa
197 ksi
1mm/min; ISO 527
BASF Ultramid® 8202C HS BK-102 PA6 (Conditioned)
Ultramid 8202C HS BK-102 is a heat stabilized, low viscosity, pigmented black, PA6, injection molding homopolymer possessing a modified crystalline structure for increased property performance and f..
Tensile Modulus 1.36 GPa
197 ksi
1mm/min; ISO 527
BASF Ultramid® 8202C HS PA6 (Conditioned)
Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also..
Tensile Modulus 1.36 GPa
197 ksi
1mm/min; ISO 527
BASF Ultramid® 8202C PA6 (Conditioned)
Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique ..
Tensile Modulus 1.36 GPa

@Temperature 80.0 °C
197 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..
Tensile Modulus 1.36 GPa

@Temperature 80.0 °C
197 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry)
Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi..