Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food contact approval EEC directive N 90/128.Example applications: Oil drum.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Water Absorption 1.9 %
1.9 %
Melt Flow 0.80 g/10 min

@Load 10.0 kg,
Temperature 235 °C
0.80 g/10 min

@Load 22.0 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 1.36 GPa
197 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Users viewing this material also viewed the following: