Polymer Property : Tensile Modulus = 0.689 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.689 GPa
100 ksi
ASTM D638
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
Tensile Modulus 0.689 - 1.03 GPa

@Temperature 23.9 °C
100 - 150 ksi

@Temperature 75.0 °F
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra..
Tensile Modulus 0.689 - 1.172 GPa
99.9 - 170.0 ksi
ASTM D638
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..