Mechanical Properties Metric English Comments
Tensile Modulus 0.689 - 1.172 GPa
99.9 - 170.0 ksi
ASTM D638
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..