Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.689 GPa | 100 ksi | ASTM D638 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.690 GPa | 100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Tensile Modulus | 0.690 GPa | 100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Tensile Modulus | 0.690 GPa | 100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Tensile Modulus | 0.689 - 1.03 GPa @Temperature 23.9 °C |
100 - 150 ksi @Temperature 75.0 °F |
|
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra.. |
|||
Tensile Modulus | 0.692 GPa | 100 ksi | Storage |
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th.. |