Mechanical Properties Metric English Comments
Tensile Modulus 0.420 GPa
60.9 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..
Tensile Modulus 0.420 GPa
60.9 ksi
1 mm/min
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and ..
Tensile Modulus 0.420 GPa
60.9 ksi
ISO 527-1/-2
DSM Arnitel® CM600-V TPC-ES FR
Extrusion, Flame Retardant (Halogen free)