Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.221 GPa | 32.0 ksi | ISO 527-2/1A/1 |
ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade) Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Ant.. |
|||
Tensile Modulus | 0.221 GPa @Temperature 120 °C |
32.1 ksi @Temperature 248 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |