ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: CompoundingFood Packaging Houseware ArticlesInjection MoldingMasterbatch Base ResinRigid Medium Sized MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 46

@Time 15.0 sec
46

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 10.3 MPa
1500 psi
ISO 527-2/1A/50
Elongation at Break 120 %
120 %
ISO 527-2/1A/50
Tensile Modulus 0.221 GPa
32.0 ksi
ISO 527-2/1A/1
Thermal Properties Metric English Comments
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 92.8 °C
199 °F
ISO 306