Tensile Strength, Yield 12.0 - 67.0 MPa
1740 - 9720 psi
Average value: 37.9 MPa Grade Count:7
Overview of materials for ABS/Polyurethane Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr..