Polymer Property : Tensile Strength, Yield = 95000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 655 MPa
95000 psi
Pacific Sintered Materials F-244-S(HT) High Carbon Steel Powdered Metal
Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals.
Tensile Strength, Yield 655 MPa

@Temperature -53.9 °C
95000 psi

@Temperature -65.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Hogen HM1250 Tungsten-Based Metal
Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Mi-Tech Metals Super Chatter Freeâ„¢ HD17.7 Tungsten-Based Metal
Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 655 MPa
95000 psi
5 inches; Un-Nitrided
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A)
TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr..
Tensile Strength, Yield >= 655 MPa

@Strain 0.200 %,
Diameter 6.35 mm
>= 95000 psi

@Strain 0.200 %,
Diameter 0.250 in
CWSR; DAN 2700.9
Haynes Ti-3Al-2.5V Alloy Titanium Tubing
Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 655 - 790 MPa
95000 - 115000 psi
Materion Brush 60â„¢ 3/4 HT
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte..
Tensile Strength, Yield >= 655 MPa
>= 95000 psi
MetalTek IN® 100 UNS N13100 Centri-Vac Nickel Based Alloy
Information provided by MetalTek
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature sheet after 2500 hours of 650°C exposure
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 655 - 779 MPa
95000 - 113000 psi
0.2% offset
Eagle Brass 64725 MAX251C, Spring
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Yield >= 655 MPa
>= 95000 psi
0.2% offset
Eagle Brass 70265 XP175, 3/4 Hard
Information provided by Eagle Brass Company
Tensile Strength, Yield >= 655 MPa
>= 95000 psi
0.2% offset
Eagle Brass 752 Nickel Silver 18%, Extra Spring
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Yield 655 MPa
95000 psi
Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze
This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Tensile Strength, Yield 655 MPa
95000 psi
Drawn rod and bar
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..
Tensile Strength, Yield 655 MPa
95000 psi
CMW® THERMKON® 65M Molybdenum Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322)
Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Grade 9 Titanium (UNS R56320)
Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy
Uses: Pump and drive shafts, impellers, valve components, springs, fasteners, oil well packers, subsurface safety valves.Property values are for samples in the metallurgical condition: 1600°F annea..
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 1149°C (2100°F) + Age
Data provided by Allvac.Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools.