Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze , Copper Casting Alloy
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Mechanical Properties Metric English Comments
Tensile Strength 862 MPa
125000 psi
Tensile Strength, Yield 655 MPa
95000 psi
Elongation at Break 2.0 %
2.0 %
Component Elements Properties Metric English Comments
Aluminum, Al 10.5 - 11.5 %
10.5 - 11.5 %
Copper, Cu >= 74.5 %
>= 74.5 %
Iron, Fe 4.0 - 5.5 %
4.0 - 5.5 %
Lead, Pb <= 0.030 %
<= 0.030 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 4.2 - 6.0 %
4.2 - 6.0 %
Other, total 0.20 %
0.20 %
Silicon, Si <= 0.15 %
<= 0.15 %
Tin, Sn <= 0.25 %
<= 0.25 %
Zinc, Zn <= 0.30 %
<= 0.30 %
Copyright © lookpolymers.com All Rights Reserved