Mechanical Properties Metric English Comments
Tensile Strength, Yield 950 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
Typical, Longitudinal Direction
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel
Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially ..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %
138000 psi

@Strain 0.200 %
Typical, Longitudinal Direction
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability
Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %,
Temperature 95.0 °C
138000 psi

@Strain 0.200 %,
Temperature 203 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 950 MPa

@Strain 0.200 %,
Temperature 550 °C
138000 psi

@Strain 0.200 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
Tensile Strength, Yield 950 - 1250 MPa

@Strain 0.200 %
138000 - 181000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1200 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..
Tensile Strength, Yield 950 MPa
138000 psi
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 950 MPa
138000 psi
ThyssenKrupp SECURE 400 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.App..
Tensile Strength, Yield 950 MPa
138000 psi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2
Information provided by HexCel
Tensile Strength, Yield >= 950 MPa

@Strain 0.200 %
>= 138000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield 950 - 1200 MPa
138000 - 174000 psi
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..