Tensile Strength, Yield 45.0 - 65.0 MPa
6530 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Tensile Strength, Yield 40.0 - 65.0 MPa
5800 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Tensile Strength, Yield 45.0 - 65.0 MPa
6530 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Tensile Strength, Yield 45.0 - 65.0 MPa
6530 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Tensile Strength, Yield 40.0 - 65.0 MPa
5800 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Tensile Strength, Yield 45.0 - 65.0 MPa
6530 - 9430 psi
Compression; ISO 527
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Tensile Strength, Yield 13.0 - 65.0 MPa
1890 - 9430 psi
Average value: 41.4 MPa Grade Count:92
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Tensile Strength, Yield 60.0 - 65.0 MPa
8700 - 9430 psi
Average value: 63.1 MPa Grade Count:17
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Tensile Strength, Yield 64.0 - 65.0 MPa
9280 - 9430 psi
ASTM D638
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/..
Tensile Strength, Yield 35.0 - 65.0 MPa
5080 - 9430 psi
Average value: 50.0 MPa Grade Count:13
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..