Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.30 MPa | 914 psi | ASTM D412 |
Polymax® Maxelast® S4670 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | -10% change after 70 hours @ 204°C; ASTM D412 |
Precision Polymer Engineering F60A Fluorosilicone Rubber Blue Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 60... |
|||
Tensile Strength, Yield | 6.30 - 11.7 MPa | 914 - 1700 psi | ±30% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering J70M Butyl Rubber Bromobutyl Rubber, 65-75 IRHD. Brominated isobutylene-isoprene copolymer. To meet BS3227 Grade 70 and ASTM D2000 line call-out MBA708, F17.Applications: Bromobutyl is resistant to the same fluids a.. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | -30% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering P60B Polyacrylate Rubber Polyacrylic or Polyacrylate Rubber, 55-65 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi.. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | -30% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering P90B Polyacrylate Rubber Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi.. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | -30% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S70B Silicone Rubber Black Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and .. |
|||
Tensile Strength, Yield | 6.30 MPa @Strain 100 % |
914 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® W DP 85786A Polyurethane Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coa.. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8450 Polyolefin Elastomer Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Tensile Strength, Yield | 6.30 MPa | 914 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8402 Polyolefin Elastomer Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 pr.. |