Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering F60A Fluorosilicone Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering F60A Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blue Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 60.Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
°IRHD; ASTM D1415
64
64
°IRHD, +2 change after 70 hours @ 204°C; ASTM D1415
Tensile Strength, Yield 6.30 MPa
914 psi
-10% change after 70 hours @ 204°C; ASTM D412
7.00 MPa
1020 psi
ASTM D412
Elongation at Break 200 %
200 %
-20% change after 70 hours @ 204°C; ASTM D412
250 %
250 %
ASTM D412
Compression Set 18 %
18 %
22 hours @ 204°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-57.0 °C
-70.6 °F
TR10
Flash Point >= 300 °C
>= 572 °F