Polymer Property : Tensile Strength, Yield = 9.915 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.915 MPa
1438 psi
Post Cure 180°F, 24h
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System
Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease..
Tensile Strength, Yield 9.915 MPa
1438 psi
Post Cure 180°F, 24h
Reltek BONDiT™ B-45TH Adhesive, Sealant & Coating System
Key Properties: Excellent adhesion to low surface energy plastics without primer.Bonding dissimilar materials.Chemical and shock resistance.Ease of use.Applications: Bonds difficult-to-bond substrat..