Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reltek BONDiT™ B-45TH Adhesive, Sealant & Coating System

Category Polymer , Adhesive , Thermoset
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ B-45TH Adhesive, Sealant & Coating System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties: Excellent adhesion to low surface energy plastics without primer.Bonding dissimilar materials.Chemical and shock resistance.Ease of use.Applications: Bonds difficult-to-bond substrates and dissimilar materials such as UHMW, polyethylene and acetal (Delrin) to steel, wood, plastics, rubber, urethane and concrete. Survives harsh environments, particularly moisture, marine and sub sea. Exceptional performance as a universal adhesive for industrial applications. Will cure underwater. Can be applied to oily surfaces. Ambient 24 hour or accelerated thermal cure.
Physical Properties Metric English Comments
Oil Absorption <= 1.0 %
<= 1.0 %
60 days ambient, Isopar M
Water Absorption <= 1.0 %
<= 1.0 %
90 days ambient DI water
Viscosity 2500 cP
2500 cP
Thrixotropic
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.804 MPa
1422 psi
Post Cure 180°F, 24h
Tensile Strength, Ultimate 9.915 MPa
1438 psi
Peak; Post Cure 180°F, 24h
Tensile Strength, Yield 9.915 MPa
1438 psi
Post Cure 180°F, 24h
Elongation at Break 130 %
130 %
Post Cure 180°F, 24h
Elongation at Yield 130 %
130 %
Post Cure 180°F, 24h
Processing Properties Metric English Comments
Cure Time 240 min
4.00 hour
Ambient Set
720 min
12.0 hour
Ambient, tack free
1440 min
24.0 hour
Ambient, 95% cure
240 min

@Temperature 65.6 °C
4.00 hour

@Temperature 150 °F
98% cure
Pot Life 30 - 40 min
30 - 40 min
Ambient
Descriptive Properties Value Comments
Color Clear with haze/slight amber