Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.90 MPa | 1440 psi | -10% change after 168 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N80N Nitrile Rubber Nitrile Rubber, 76-85 °IRHD. Copolymer of acrylonitrile and butadiene. Meets Aerospace Specification DTD5595A Grade 80. ASTM designation = NBR. ISO designation = NBR.Applications: Sealing petroleum.. |
|||
Tensile Strength, Yield | 9.90 MPa | 1440 psi | 10% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V75G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 70-80 °IRHD. Diesel liner ring grade. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK707, A1-10, B38, EF31, EO78, F.. |
|||
Tensile Strength, Yield | 9.90 MPa | 1440 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Tensile Strength, Yield | 9.90 MPa | 1440 psi | |
Dow LDPE 993I Low Density Polyethylene DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability .. |