Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.93 MPa
1440 psi
ASTM D412
Polymax® Maxelast® C4860 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 9.93 MPa
1440 psi
ASTM D412
Polymax® Maxelast® C4870 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 9.94 MPa
1440 psi
-29% change after 72 hours @ 70°C; ASTM D412
Precision Polymer Engineering B60B Styrene Butadiene Rubber
Styrene-Butadiene Rubber (SBR) 55-65 °IRHD. Copolymer of styrene and butadiene.Applications: Good sealing resistance to brake fluids and water. Poor against petroleum oils, solvents and weather. ..
Tensile Strength, Yield 9.90 MPa
1440 psi
-10% change after 168 hours @ 100°C; ASTM D412
Precision Polymer Engineering N80N Nitrile Rubber
Nitrile Rubber, 76-85 °IRHD. Copolymer of acrylonitrile and butadiene. Meets Aerospace Specification DTD5595A Grade 80. ASTM designation = NBR. ISO designation = NBR.Applications: Sealing petroleum..
Tensile Strength, Yield 9.90 MPa
1440 psi
10% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V75G Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 70-80 °IRHD. Diesel liner ring grade. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK707, A1-10, B38, EF31, EO78, F..
Tensile Strength, Yield 9.93 MPa
1440 psi
Change in tensile strength after 168 hours at 176°F; ASTM D638
Teknor Apex Sinvicomp SIM 5000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield >= 9.93 MPa
>= 1440 psi
Heat Aging (7 days at 121°C); ASTM D412
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation
Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of..
Tensile Strength, Yield 9.90 MPa
1440 psi
after aging 1 week @ 135°C; ASTM D638
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding
E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel..
Tensile Strength, Yield 9.90 MPa
1440 psi
Dow LDPE 993I Low Density Polyethylene
DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability ..