Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.31 MPa | 1350 psi | 510 mm/min; ASTM D412A |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 8103 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive Interior PartsInformation .. |
|||
Tensile Strength, Yield | >= 9.31 MPa | >= 1350 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7182E Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D412 |
Teknor Apex APEX® 3211-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 6704 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 10706 Wire & Cable Flexible PVC Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.31 MPa | 1350 psi | ASTM D-638 |
Axiall 4750 Flexible PVC General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 9.31 MPa @Strain 300 % |
1350 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-5145D Thermoplastic Elastomer - SBC