Axiall 10706 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 10706 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 73
67 - 73
delayed; ASTM D-2240
Tensile Strength, Yield 9.31 MPa
1350 psi
ASTM D-638
Elongation at Yield 365 %
365 %
ASTM D-638
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638