Material Notes:
An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.21 - 1.25 g/cc
1.21 - 1.25 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 69
63 - 69
delayed; ASTM D-2240
Tensile Strength, Yield 9.31 MPa
1350 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 171 °C
340 °F