Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.90 - 9.10 MPa
711 - 1320 psi
±30% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering C90B Chloroprene Rubber
Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu..
Tensile Strength, Yield 4.90 MPa

@Strain 100 %
711 psi

@Strain 100 %
ASTM D412
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Tensile Strength, Yield 4.90 MPa

@Treatment Temp. 70.0 °C,
Time 252000 sec
711 psi

@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber
Two Material Product:Material 1: VicoSeal™ 003R-30 DUROMaterial 2: 11 ga CRS yellow anodized natural rubber vulcanized to yellow anodized steel (RoHS Approved)Information provided by Vicone
Tensile Strength, Yield 4.90 MPa
711 psi
at 100% elongation; ASTM D412
Lubrizol Estane® CR180A Thermoplastic Polyurethane
Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..
Tensile Strength, Yield 4.90 MPa
711 psi
at 100% elongation; ASTM D412
Lubrizol Estane® R180A Thermoplastic Polyurethane
Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi..
Tensile Strength, Yield 4.90 MPa
711 psi
ASTM D412
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to ..