Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.90 - 9.10 MPa | 711 - 1320 psi | ±30% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering C90B Chloroprene Rubber Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu.. |
|||
Tensile Strength, Yield | 4.90 MPa @Strain 100 % |
711 psi @Strain 100 % |
ASTM D412 |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength, Yield | 4.90 MPa @Treatment Temp. 70.0 °C, Time 252000 sec |
711 psi @Treatment Temp. 158 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber Two Material Product:Material 1: VicoSeal™ 003R-30 DUROMaterial 2: 11 ga CRS yellow anodized natural rubber vulcanized to yellow anodized steel (RoHS Approved)Information provided by Vicone |
|||
Tensile Strength, Yield | 4.90 MPa | 711 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® CR180A Thermoplastic Polyurethane Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 4.90 MPa | 711 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tensile Strength, Yield | 4.90 MPa | 711 psi | ASTM D412 |
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to .. |